Publication: Investigation on the performance of coal fly ash based polymer gel for water control.
| datacite.subject.fos | oecd::Engineering and technology::Chemical engineering | |
| dc.contributor.author | Adewunmi, Ahmad Akanbi | |
| dc.date.accessioned | 2026-11-16T04:07:20Z | |
| dc.date.available | 2026-11-16T04:07:20Z | |
| dc.date.issued | 2017-07 | |
| dc.description.abstract | This research was conducted to investigate the performance of coal fly ash (CFA) based polymer gels developed from polyacrylamide (PAM) polymer and polyethyleneimine (PEI) crosslinker for water control in mature oil fields. The constant failure of water shutoff polymer gels owing to their inappropriate gelation time, weak gel strength, thermal instability, syneresis effect, coupled with the heterogeneous nature of oil wells have necessitated constant development of new crosslinked polymer gels to tackle excessive water production challenges during enhanced oil recovery (EOR) applications. In this research, pure PAM/PEI gel and various PAM/PEI-CFA composite gels from CFA (0.5 to 2 wt%), PAM (2.87 to 8.4 wt%) and PEI (0.3 to 1.04 wt%) were developed and characterized. The CFA acts as a reinforcing inorganic filler. Experimental results revealed that gelation mechanism of PAM/PEI gel occurred through the substitution reaction. The synergistic effects between CFA and PAM/PEI gels structural network was confirmed by the X-ray diffraction (XRD) instrument. Gelation time values investigated at temperature of 90 °C for the pure PAM/PEI gel and various PAM/PEI-CFA composite gels were found to be within 3.5 to 120 hours. Short gelation time value (3.5 to 4.5 hours) is suitable for near wellbore treatment while long gelation time value (120 hours) is appropriate for deep reservoir treatment. Findings from the viscoelastic behavior measurements at temperature of 90 °C and specific periods during gelation performance showed that PAM/PEI-CFA composite gels achieved enhanced strength as compared to the pure PAM/PEI gel. The PAM/PEI-CFA composite gel formulated from 6 wt% PAM, 0.67 wt% PEI, and 2 wt% CFA produced the optimal strength values: elastic modulus G´ = 3559.710 Pa, and viscous modulus G´´ = 1690.771 Pa. Thermal results showed that various PAM/PEI-CFA composite gels have better thermal resilience than the pure PAM/PEI gel. Syneresis rate of pure PAM/PEI gel was found to be less than 4% and various PAM/PEI-CFA composite gels syneresis rates were estimated to be within the range of 2% to 19%. Permeability tests showed that PAM/PEI-CFA composite gel effectively reduced the brine permeability by 90 %. Support vector regression (SVR) computational tool was applied to predict the experimental thermal findings of pure PAM/PEI gel and PAM/PEI-CFA composite gels filled with various CFA amounts. Estimated thermal results conformed well to the experimental thermal data. Predicted results indicate that CFA within 2 wt% is suitable for PAM/PEI-CFA composite gel optimal performance during EOR applications. | |
| dc.identifier.uri | https://erepo.usm.my/handle/123456789/25468 | |
| dc.language.iso | en | |
| dc.title | Investigation on the performance of coal fly ash based polymer gel for water control. | |
| dc.type | Resource Types::text::thesis::doctoral thesis | |
| dspace.entity.type | Publication | |
| oairecerif.author.affiliation | Universiti Sains Malaysia |