Publication: Electrophoretically deposited carbon nanotubes based thermal interface materials for heat removal.
Loading...
Date
2017-08
Authors
Bahru, Raihana
Journal Title
Journal ISSN
Volume Title
Publisher
Abstract
Recently, electronic system becomes more complex with the power density in the electronic design is increased and components generate more energy which eventually leads to the overheating of the electronic device. This lead to the application of TIM to remove heat from the electronic device where the TIM required materials with higher thermal conductivity. Therefore, this study focuses on the development of carbon nanotubes (CNTs) which have high thermal conductivity based thermal interface materials (TIM) by using electrophoretic deposition (EPD) method. The as-produced CNTs synthesized via catalytic chemical vapor deposition (CCVD) method was purified and dispersed in solvents to obtain good suspension. The solvents selected for CNTs suspension are distilled water and organic solvents (mixture of acetone and ethanol, dimethylformamide (DMF), N-methyl-2 pyrrolidone (NMP) and texanol). The analyses for the suspension stability was verified using zetasizer. The parameters of EPD process studied were solution concentration (0.1 – 1.0 mg/ml), voltage applied (100 – 200 V), deposition time (1 – 20 minutes) and gap between electrodes (10 – 20 mm) towards the mass of deposited CNTs. The range of CNTs suspension concentration studied was 0.1 – 1.0 mg/ml and the 0.5 mg/ml suspension concentration gavemaximum thickness of 11.98 µm CNTs deposition. The EPD method conducted at room temperature and atmospheric pressure with supply of direct current on nickel plated copper substrate as heat spreader. The parameters were studied on individual effect and further studied using Response of Surface Methodology (RSM) on the mass of CNTs deposited. The optimum process condition of EPD is 175V applied voltage, 10 minutes deposition time and 10 mm gap of electrodes which enabled the deposition of 1.6 mg of CNTs with thickness of 14.14 µm. The surface morphology and thickness of deposited CNTs was characterized using scanning electron microscopy (SEM) and the deposition mechanism of EPD was studied. For the fabrication of TIM, the deposition process was repeated and the maximum thickness of deposited CNTs was observed at 56.95 µm for 6 layers. The result obtained fulfilled the minimum thickness requirement of TIM of 50.00 µm. The thermal properties of the 6 layers CNTs based TIM were characterized to be thermal conductivity of 27.08 W/m.K, thermal diffusivity of 2.09 mm2/s and heat capacity of 1712.01 J/kg.K. The heat removalprocess of CNTs based TIM was modeled using Computational Solution (COMSOL) simulation to provide the clear view on heat transfer process among materials by using the thermal properties measured from experiments. The thermal conductivity predicted by COMSOL for 6 layers CNTs and heat spreader were 45.26 and 5.88 W/m.K, respectively. The CNTs based TIM temperature can be reduced from 373.00 K to 348.28 K with heat flux in average of 58108.70 W/m2.These results indicated that CNTs is a good material for fabrication of TIM for efficient heat removal from microelectronic devices.